    What effect would age hardening at 700C for 8 hours have on a part made from MIM 17-4 PH have? This is the only call out on the drawing provided for a part we received. Thank you Jim

  2. #2
    Technical Fellow Kelly_Bramble's Avatar
    Join Date
    Feb 2011
    Location
    Bold Springs, GA
    Posts
    2,625
    See page 5-6 of the following attachment..